| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 55 | 55 | ASTM D2240 |
| Tensile Stress | 3.79 MPa @Strain 100 % |
550 psi @Strain 100 % |
510 mm/min; ASTM D412A |
| Tensile Strength, Yield | 9.31 MPa | 1350 psi | 510 mm/min; ASTM D412A |
| Elongation at Break | 390 % | 390 % | 510 mm/min; ASTM D412A |
| Tear Strength | 22.8 kN/m | 130 pli | Die C, 2 in/min; ASTM D1004 |
| Compression Set | 10 % @Temperature 23.0 °C, Time 79200 sec |
10 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.0372 GPa @Temperature -35.0 °C |
5.40 ksi @Temperature -31.0 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -47.2 °C | -53.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
| 177 - 193 °C | 351 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Low Gloss | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |