Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible Y126 White 317 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible C90A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible XV3830B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 204 °C | 350 - 400 °F | Extrusion |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Melt Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Melt Temperature | 177 - 185 °C | 351 - 365 °F | |
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R276AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to pro.. |
|||
Melt Temperature | 177 °C | 350 °F | |
LyondellBasell Petrothene® NA952000 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Melt Temperature | 177 °C | 350 °F | |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Melt Temperature | 177 °C | 350 °F | |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Spartech E65080 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Teknor Apex APEX® 3302-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Teknor Apex APEX® 90-A472R-75-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Melt Temperature | 177 - 227 °C | 350 - 440 °F | |
Ecomass® 3608TU96 Tungsten Filled Polyethylene Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers |
|||
Melt Temperature | 177 - 227 °C | 350 - 440 °F | |
Ecomass® 3620BX60 18% Borated Polyethylene (HDPE) 18% Borated Polyethylene (HDPE), Product Form - Pellets, No Pre-Drying RequiredProcessing Method: Injection Molding, Compression MoldingNeutron Shielding ApplicationsInformation provided by Technic.. |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Melt Temperature | 177 - 204 °C | 350 - 400 °F | Extrusion |
ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Melt Temperature | 177 - 204 °C | 350 - 400 °F | Extrusion |
ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Melt Temperature | 177 - 204 °C | 350 - 400 °F | |
ExxonMobil Santoprene® 9101-80E Thermoplastic Vulcanizate - Co-extrusion Product Description: A black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for coextrusion applications, particularly for the static foot of.. |
|||
Melt Temperature | 177 °C | 351 °F | Extrusion |
Dow Tyrin® 3611P Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 971 Wire & Cable Flexible PVC Matte-finish, CL2 jacket compound rated for 90°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 13821 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 873 Wire & Cable Flexible PVC 80°C rated, low migratory, oil resistant coil cord jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 19740 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Informa.. |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |