Polymer Property : Melt Temperature = 182 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Melt Temperature 182 - 193 °C
360 - 379 °F
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Melt Temperature 182 - 193 °C
360 - 379 °F
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Melt Temperature 182 - 193 °C
360 - 379 °F
PolyOne Geon™ L4605 Green 5765 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Melt Temperature 182 - 199 °C
360 - 390 °F
M. Holland Company LD225 LDPE  (discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, High Clarity, High Gloss, Heat Sealable, Good Processability, Medium SlipUses: FilmProcessing Method: Blown FilmInformation pro..
Melt Temperature 182 - 193 °C
360 - 379 °F
Huntsman PE1504 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Melt Temperature 182 - 221 °C
360 - 430 °F
Injection Molding
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Westlake EF421 Low Density Polyethylene
WESTLAKE polyethylene EF421 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and general purpose food packaging app..
Melt Temperature 182 - 210 °C
360 - 410 °F
Molding
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha..
Melt Temperature 182 °C
360 °F
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..
Melt Temperature 182 °C
360 °F
Axiall 8743 Moldings & Extrusions Flexible PVC
A high quality extrusion compound recommended for weatherstrips, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 182 °C
360 °F
Axiall 8900 Moldings & Extrusions Flexible PVC
General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 182 °C
360 °F
Axiall 8922 Moldings & Extrusions Flexible PVC
A general purpose, matte finish, extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 182 - 220 °C
360 - 428 °F
Average value: 204 °C Grade Count:14
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Melt Temperature 182 - 199 °C
360 - 390 °F
Molding
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l..