| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 91 | 91 | ASTM D2240 |
| Tensile Stress | 11.7 MPa <br>@Strain 100 % |
1700 psi <br>@Strain 100 % |
510 mm/min; ASTM D412A |
| Tensile Strength, Yield | 18.6 MPa | 2700 psi | 510 mm/min; ASTM D412A |
| Elongation at Break | 350 % | 350 % | 510 mm/min; ASTM D412A |
| Tear Strength | 60.4 kN/m | 345 pli | Die C, 510 mm/min; ASTM D624 |
| Clash Berg Modulus | 0.483 GPa | 70.1 ksi | ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -34.4 °C | -29.9 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |