Polymer Property : Melt Temperature = 370 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 188 - 210 °C
370 - 410 °F
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE)
Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan..
Melt Temperature 188 - 199 °C
370 - 390 °F
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Melt Temperature 188 - 199 °C
370 - 390 °F
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL EF-6133L2 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-101 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-102 BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-1155A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-1424A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-1434A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-1488G Thermoplastic Elastomer
Uses: Flexible Grips; General Purpose; Handles; Household Goods; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-2460B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-2503S Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-2540A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-2572A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-6045 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-2468A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Temperature 188 - 232 °C
370 - 450 °F
Clariant Renol CAB1000 Cellulose Acetate Butyrate
Data provided by Clariant Masterbatches
Melt Temperature 188 °C
370 °F
Axiall 8621 Moldings & Extrusions Flexible PVC
High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia ..
Melt Temperature 188 °C
370 °F
Axiall 16860 Wire & Cable Flexible PVC
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 188 °C
370 °F
Axiall 19912 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C rated insulation compound recommended for various style # applications including 1007 and 1015. The compound is formulated for microbial and fungal resistance.Informatio..
Melt Temperature 188 °C
370 °F
Axiall 8933 Moldings & Extrusions Flexible PVC
General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 188 - 193 °C
370 - 379 °F
PolyOne Geon™ Vinyl Wire & Cable W1201 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 188 - 210 °C
370 - 410 °F
Stock
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated  (discontinued **)
Data provided by PolyOne.