Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 85880 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87717 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87727 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L9620 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJAX204V Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 193 °C | 339 - 379 °F | ASTM D789 |
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 171 - 193 °C | 339 - 379 °F | ASTM D789 |
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Flexible R881C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 193 °C | 370 - 379 °F | |
PolyOne Geon™ Vinyl Flexible XV3581G Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
Huntsman PE 1008 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Flexible R277AM Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
Huntsman PE1205 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK11 Styrene-Butadiene Copolymer, Film Grade Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: Provides the same high performance film properties as.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L5880 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 185 - 193 °C | 365 - 379 °F | |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i.. |