Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical KEYFLEX TO1065A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID HI1202B(W) PA66, High Impact Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID LW4303B(W) PA66+MF30%, Low Warpage Feature: Injection Molding, PA66+MF30%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HG3100 PP+MF10%, High Gloss Description: Injection Molding, PP+MF10%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5204G PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5302A PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP2300 PP+GF30% Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical KEYFLEX TO1075AR Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |