Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Extrusion |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Injection Molding |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Extrusion |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion Molding |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer Description: Stat-Rite® E-1140 is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1140 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to .. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy sys.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD .. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
DuPont Performance Polymers Hytrel® 4068FG TPC-ET
(Unverified Data**) Hytrel® 4068FG is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |