Polymer Property : Drying Temperature = 76.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 76.0 °C
169 °F
NYCOA 1417HS PA 6
impact modified, heat stabilized, medium high impact strengthInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 1838 Copolymer Nylon Alloy
good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2001 PA 6
high melt strength general extrusion and molding grade of nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2011 Copolymer Nylon
impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2012 Copolymer Nylon
easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2037 15% Glass Filled Nylon 6
15% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2038 10% Glass Filled Nylon 6
10% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2046 Copolymer Nylon 6/69
extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2047 Copolymer Nylon 6/69
extrusion, high melt viscosity. & strength., low crystallinity Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2061 Copolymer Nylon 6/69
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2062 Copolymer Nylon 6/66
FDA approved extrusion grade for film.Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2084 HS PA 6
lubricated flexible tubing and conduitInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2237 Copolymer Nylon 6/66 Alloy
transparent molding and extrusion gradeInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 2263 Copolymer Nylon Alloy
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 27/300I Glass Filled Nylon 6
30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 27/300SR Glass Filled Nylon 6
30% glass filled, flame retardant to UL 94 H-B nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 27/330KNF Glass Filled Nylon 6
33% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 27/440KNF Glass Filled Nylon 6
44% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 400 PA 6
nucleated general molding gradeInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 436 PA 6
NSF rated general purpose molding gradeInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 446 PA 6
UL-94 V-2 rated for flammability extrusion grade for rod, sheet and filmInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 512 PA 6
UL and NSF rated nucleated general purpose molding gradeInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 534H PA 6
high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and moldingInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 567 PA 6
plasticized general purpose molding and extrusion grade used in shoe heels and mono.Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 578 PA 6
very high viscosity molding & extrusion grade for tubing, pipes, film and tapesInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 589 PA 6
FDA approved molding, extrusion and blown film gradeInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 715C PA 6
plasticized, high viscosity extrusion grade for monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 7551 Copolymer Nylon Alloy
resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
NYCOA 870 PA 6
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 3,000 fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Drying Temperature 76.0 °C
169 °F
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..