Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NYCOA 2011 Copolymer Nylon

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF NYCOA 2011 Copolymer Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Yield Strength 22.0 MPa
3190 psi
ASTM D790
Flexural Modulus 0.468 GPa
67.9 ksi
ASTM D790
Izod Impact, Notched 1.75 J/cm
3.28 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 205 °C
401 °F
ASTM D789
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 210 °C
410 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Drying Temperature 76.0 °C
169 °F
Users viewing this material also viewed the following: