Material Notes:
high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and moldingInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break >= 130 %
>= 130 %
ASTM D638
Flexural Yield Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 2.689 GPa
390.0 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 220 °C
428 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F