| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | NYCOA, Inc. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | NYCOA 567 PA 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183-A |
| Water Absorption | 3.1 % | 3.1 % | ISO METHOD 62 |
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 66.0 MPa | 9570 psi | ISO METHOD 527 |
| Elongation at Break | >= 300 % | >= 300 % | ISO METHOD 527 |
| Flexural Yield Strength | 47.0 MPa | 6820 psi | ISO METHOD 178 |
| Flexural Modulus | 0.965 GPa | 140 ksi | ISO METHOD 178 |
| Izod Impact, Notched | 1.56 J/cm | 2.92 ft-lb/in | ISO METHOD 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | ISO METHOD 3146C |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 °C | 482 °F | |
| Rear Barrel Temperature | 220 °C | 428 °F | |
| Middle Barrel Temperature | 230 °C | 446 °F | |
| Front Barrel Temperature | 250 °C | 482 °F | |
| Nozzle Temperature | 250 °C | 482 °F | |
| Mold Temperature | 80.0 °C | 176 °F | |
| Drying Temperature | 76.0 °C | 169 °F |