| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled |
| Manufacturer | NYCOA, Inc. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | NYCOA 2038 10% Glass Filled Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
| Elongation at Break | 10 % | 10 % | ASTM D638 |
| Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
| Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 216 °C | 421 °F | ASTM D789 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 °C | 482 °F | |
| Rear Barrel Temperature | 215 °C | 419 °F | |
| Middle Barrel Temperature | 230 °C | 446 °F | |
| Front Barrel Temperature | 250 °C | 482 °F | |
| Nozzle Temperature | 250 °C | 482 °F | |
| Mold Temperature | 80.0 °C | 176 °F | |
| Drying Temperature | 76.0 °C | 169 °F |