Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry Product Description: Glass Fiber (60% Reinforced), Nylon 6 injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents, Lubricants and Heat Stabiliz.. |
|||
Rear Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 288 - 288 °C | 550 - 550 °F | |
Star Plastics PC701 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 288 - 288 °C | 550 - 550 °F | |
Star Plastics PC703 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC743 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |