Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |