Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material exceeds the performance required by the automotive industry for polymeric materials exposed to antifreeze at 226°F (108°C), even when tested at 275°F (135°C).Features: Antifreeze Resistant; Glycol Resistant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High StrengthUses: Automotive Applications; Automotive Under the Hood; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D6779 PA121G45; FORD WSS-M4D997-A Color: BK-324 Black; GM GMP.PPA.018 Color: Black; GM GMW16360P-PPA-GF45 Color: Black; IMDS ID 14880200 Color: BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183
Filler Content 45 %
45 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4
0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4
0.0060 cm/cm
0.0060 in/in
Type D2; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 244 MPa
35400 psi
ISO 527-2
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Flexural Strength 335 MPa
48600 psi
ISO 178
Flexural Yield Strength 359 MPa
52100 psi
ASTM D790
Flexural Modulus 12.6 GPa
1830 ksi
ISO 178
13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
Type 1, Notch A; ISO 180
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
Type 1, Edgewise; ISO 179
Thermal Properties Metric English Comments
Melting Point 312 °C
594 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 282 °C
540 °F
Unannealed; Flatwise; ISO 75-2/A
282 °C
540 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 79.4 °C
175 °F
Hopper
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant