Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stability, chemical resistance and ductility. This resin has a high heat deflection temperature and a high flexural modulus, with greater tensile elongation than untoughened glass reinforced PPA.Features: Good Chemical Resistance; Good Dimensional Stability; Heat Stabilized; High Heat Resistance; Impact ModifiedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Bobbins; Connectors; General Purpose; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal ReplacementInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PPA0111 G17 KD124 KN055 PN046 YI238 LD002 Color: BK 324 Black; ASTM D4000 PPA0111 G17 KD124 KN055 PN046 YI238 LD002 Color: NT Natural; ASTM D6779 PA123G15 YI220; GM GMN6828 Color: BK 324 Black; GM GMN6828 Color: NT Natural; GM GMP.PPA.009 Color: BK 324 Black; GM GMP.PPA.009 Color: NT Natural; GM GMW15702-021991 Color: BK 324 Black; GM GMW15702-021991 Color: NT Natural; GM GMW16359P-PPA-GF15 Color: BK 324 Black; GM GMW16359P-PPA-GF15 Color: NT Natural; ISO 1874-PA 6T/6I/66-HI, MH, 12-060, GF16; YAZAKI YPES-25-02-305 Color: BK 324 Black; YAZAKI YPES-25-02-305 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
Filler Content 16 %
16 %
Glass Fiber
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.5 MPa

@Temperature 100 °C
9500 psi

@Temperature 212 °F
2; ISO 527-2
160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
2; ISO 527-2
Tensile Strength 161 MPa
23400 psi
ASTM D638
Elongation at Break 3.8 %
3.8 %
ASTM D638
3.7 %

@Temperature 23.0 °C
3.7 %

@Temperature 73.4 °F
ISO 527-2
4.2 %

@Temperature 100 °C
4.2 %

@Temperature 212 °F
ISO 527-2
Tensile Modulus 6.48 GPa
940 ksi
ASTM D638
6.69 GPa

@Temperature 100 °C
970 ksi

@Temperature 212 °F
2; ISO 527-2
6.89 GPa

@Temperature 23.0 °C
999 ksi

@Temperature 73.4 °F
2; ISO 527-2
Flexural Strength 226 MPa
32800 psi
ASTM D790
141 MPa

@Temperature 100 °C
20500 psi

@Temperature 212 °F
2; ISO 178
197 MPa

@Temperature 23.0 °C
28600 psi

@Temperature 73.4 °F
2; ISO 178
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
4.96 GPa

@Temperature 100 °C
719 ksi

@Temperature 212 °F
ISO 178
6.69 GPa

@Temperature 23.0 °C
970 ksi

@Temperature 73.4 °F
ISO 178
Compressive Strength 124 MPa
18000 psi
ASTM D695
Shear Strength 69.6 MPa
10100 psi
ASTM D732
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.60 J/cm
18.0 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 53.0 kJ/m²
25.2 ft-lb/in²
Type 1; ISO 180
Charpy Impact Unnotched 8.60 J/cm²
40.9 ft-lb/in²
Type 1, Edgewise; ISO 179
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
Type 1, Edgewise; ISO 179
Dart Drop, Total Energy 10.0 J
7.38 ft-lb
Instrumented; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 100 - 200 °C
8.89 µin/in-°F

@Temperature 212 - 392 °F
2
22.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.2 µin/in-°F

@Temperature 32.0 - 212 °F
2
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature 0.000 - 100 °C
41.7 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
120 µm/m-°C

@Temperature 100 - 200 °C
66.7 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Melting Point 310 °C
590 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 268 °C
514 °F
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
Annealed; ASTM D648
258 °C
496 °F
Unannealed; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 110 °C

@Time 14400 sec
230 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: