| Category | Polymer , Thermoplastic , Polyphthalamide (PPA) |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183/A |
| Filler Content | 45 % | 45 % | Glass Fiber Reinforcement |
| Water Absorption | 0.12 % @Time 86400 sec |
0.12 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | Conditioned; ASTM D955 |
| 0.0020 cm/cm | 0.0020 in/in | ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.0010 cm/cm | 0.0010 in/in | Conditioned; ASTM D955 |
| 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 125 | 125 | R-Scale; ASTM D785 |
| Tensile Strength at Break | 228 MPa | 33100 psi | Conditioned; ASTM D638 |
| 259 MPa | 37600 psi | ASTM D638 | |
| 263 MPa | 38100 psi | ISO 527-2 | |
| Elongation at Break | 2.1 % | 2.1 % | Conditioned; ASTM D638 |
| 2.6 % | 2.6 % | ASTM D638 | |
| 2.7 % | 2.7 % | ISO 527-2 | |
| Tensile Modulus | 16.0 GPa | 2320 ksi | ISO 527-2 |
| 17.2 GPa | 2490 ksi | Conditioned; ASTM D638 | |
| 17.2 GPa | 2490 ksi | ASTM D638 | |
| Flexural Strength | 376 MPa | 54500 psi | ISO 178 |
| Flexural Yield Strength | 294 MPa | 42600 psi | Conditioned; ASTM D790 |
| 363 MPa | 52600 psi | ASTM D790 | |
| Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
| 13.8 GPa | 2000 ksi | Conditioned; ASTM D790 | |
| 14.8 GPa | 2150 ksi | ISO 178 | |
| Compressive Strength | 302 MPa | 43800 psi | Conditioned; ASTM D695 |
| 314 MPa | 45500 psi | ASTM D695 | |
| Poissons Ratio | 0.41 | 0.41 | ASTM E132 |
| Shear Modulus | 5.67 - 6.10 GPa | 822 - 885 ksi | Calculated |
| Shear Strength | 91.7 MPa | 13300 psi | Conditioned; ASTM D732 |
| 108 MPa | 15700 psi | ASTM D732 | |
| Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | Conditioned; ASTM D256 |
| 1.20 J/cm | 2.25 ft-lb/in | ASTM D256 | |
| 13.0 J/cm | 24.4 ft-lb/in | ASTM D256 | |
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180/1A |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 11.0 µm/m-°C @Temperature 160 - 249 °C |
6.11 µin/in-°F @Temperature 320 - 480 °F |
TMA; ASTM E831 |
| 14.0 µm/m-°C @Temperature 0.000 - 100 °C |
7.78 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 | |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 0.000 - 100 °C |
27.8 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E831 |
| 100 µm/m-°C @Temperature 160 - 249 °C |
55.6 µin/in-°F @Temperature 320 - 480 °F |
ASTM E831 | |
| Melting Point | 312 °C | 594 °F | Peak; ASTM D3418 |
| 312 °C | 594 °F | ISO 11357-3 | |
| Maximum Service Temperature, Air | 165 °C @Time 7.20e+7 sec |
329 °F @Time 20000 hour |
Continuous; ASTM D3045 |
| 185 °C @Time 1.80e+7 sec |
365 °F @Time 5000 hour |
Continuous; ASTM D3045 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 301 °C @Thickness 3.18 mm |
574 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ISO 75-2/A |
| 287 °C @Thickness 3.18 mm |
549 °F @Thickness 0.125 in |
Annealed; ASTM D648 | |
| Flammability, UL94 | HB @Thickness 3.18 mm |
HB @Thickness 0.125 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | Conditioned; ASTM D257 |
| 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 | |
| Dielectric Constant | 4.4 @Frequency 1.00e+6 Hz |
4.4 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 4.5 @Frequency 1.00e+6 Hz |
4.5 @Frequency 1.00e+6 Hz |
Conditioned; ASTM D150 | |
| 4.6 @Frequency 60.0 Hz |
4.6 @Frequency 60.0 Hz |
ASTM D150 | |
| 4.9 @Frequency 60.0 Hz |
4.9 @Frequency 60.0 Hz |
Conditioned; ASTM D150 | |
| Dielectric Strength | 22.0 kV/mm | 559 kV/in | Conditioned; ASTM D149 |
| 22.0 kV/mm | 559 kV/in | ASTM D149 | |
| Dissipation Factor | 0.0050 @Frequency 60.0 Hz |
0.0050 @Frequency 60.0 Hz |
ASTM D150 |
| 0.0090 @Frequency 60.0 Hz |
0.0090 @Frequency 60.0 Hz |
Conditioned; ASTM D150 | |
| 0.016 @Frequency 1.00e+6 Hz |
0.016 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| 0.021 @Frequency 1.00e+6 Hz |
0.021 @Frequency 1.00e+6 Hz |
Conditioned; ASTM D150 | |
| Arc Resistance | 125 sec | 125 sec | Conditioned; ASTM D495 |
| 145 sec | 145 sec | ASTM D495 | |
| Comparative Tracking Index | 550 V | 550 V | UL 746 |
| 550 V | 550 V | Conditioned; UL 746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Feed Temperature | 79.4 °C | 175 °F | Hopper Temperature |
| Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
| Front Barrel Temperature | 316 - 329 °C | 601 - 624 °F | |
| Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
| Mold Temperature | 135 °C | 275 °F | |
| Drying Temperature | 121 °C | 250 °F | |
| Dry Time | 4.00 hour | 4.00 hour | |
| Moisture Content | 0.10 % | 0.10 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Heat Stabilizer | |
| Appearance | Black | |
| Natural Color | ||
| Automotive Specifications | ASTM D4000 PA121 G45 Color: BK324 Black | |
| ASTM D4000 PA121 G45 Color: NT Natural | ||
| ASTM D5336 PPA0120 G45 A06637 Color: BK324 Black | ||
| ASTM D6779 PA121G45 | ||
| BOSCH N28 BN05-OX1 BN0510-GF45-3Anf10SO Color: NT Natural | ||
| BOSCH N28 BN05-OX1 BN0510-GF45-3Asw01SO Color: BK324 Black | ||
| DELPHI DCM4889 Color: BK324 Black | ||
| DELPHI DCM4889 Color: NT Natural | ||
| DELPHI M-6073 Color: BK324 Black | ||
| FORD WSK-M4D861-A2 Color: BK324 Black |