Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 193 - 210 °C | 380 - 410 °F | |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 177 - 210 °C | 350 - 410 °F | |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical LUPOL GP3202 PP+MF20% Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Start Point: 190°C |
Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical LUPOL HI5204B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical LUPOL HM5302W PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | H1 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Aft-1. Region Temperature |
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Aft-1. Region Temperature |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Rear Barrel Temperature | 200 - 210 °C | 392 - 410 °F | |
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Aft-1. Region Temperature |
Tisan TISAKRIL® 30% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |