Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 199 - 216 °C | 390 - 420 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Rear Barrel Temperature | 199 °C | 390 °F | |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |