Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rear Barrel Temperature = 193 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral
Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP522-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black
Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 °C
380 °F
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 193 °C
380 °F
TPI Porene® ABS-GA800 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 193 °C
380 °F
TPI Porene® ABS-KU650 Super High Heat ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 193 °C
380 °F
Chi Mei Polylac® PA-747 ABS
High impact
Rear Barrel Temperature 193 °C
380 °F
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Kraton® G7720 GI-N (SEBS) Compound
Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products.