Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX TO1065A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCON TR1000 PMMA+CNT Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG .. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 80 AB Thermoplastic Polyurethane Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 85 AB Thermoplastic Polyurethane Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 92 AB Thermoplastic Polyurethane Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | c |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
Elastron® G SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |