Material Notes:
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling material for sports footwear and top-pieces. The features offered include:DurabilityExcellent surface definitionAbrasion resistanceFlex resistancePhthalate free TPU Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868
Hardness, Shore D 50
50
ISO 868
Tensile Strength at Break 35.0 MPa
5080 psi
ISO 37
Elongation at Break 425 %
425 %
ISO 37
100% Modulus 0.0130 GPa
1.89 ksi
ISO 37
300% Modulus 0.0240 GPa
3.48 ksi
ISO 37
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178
Tear Strength 146 kN/m
833 pli
ISO 34B
Abrasion 20
20
mm<sup>3</sup>; ISO 4649
Compression Set 20 %
20 %
ISO 815
Processing Properties Metric English Comments
Feed Temperature 25.0 - 35.0 °C
77.0 - 95.0 °F
Rear Barrel Temperature 190 - 200 °C
374 - 392 °F
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Front Barrel Temperature 200 - 210 °C
392 - 410 °F
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Injection Pressure 2.00 - 10.0 MPa
290 - 1450 psi
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Screw Speed 20 - 80 rpm
20 - 80 rpm
Descriptive Properties Value Comments
Compression Ratio 2-3:1
L/D Ratio 20-25:1
Ross Flex -10°C, BS 5131
Typical Screw Diameter 40-120 nm