| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical AF312 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical FH380P ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF380U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HI121U ABS
Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 405AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 406AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 410AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 460AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1045D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX TO1065A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX TO1192A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCON TR1000 PMMA+CNT
Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG ..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical SG175 ABS, Super Surface Gloss
Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf..
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Extrusion |
|
Stellarchem SE/PA745B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Rear Barrel Temperature | 185 - 200 °C | 365 - 392 °F | |
|
Chi Mei Acryrex® CM-207 PMMA
Features:General PurposeGood Weather ResistanceHigh GlossHigh Heat ResistanceHigh StrengthMedium ViscosityUses: Automotive Interior PartsBathroom AccessoriesContainersCosmeticsHousehold GoodsKnobsRo..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF350U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane
Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi..
|
|||