| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
|
|||
| Mold Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Injection Molding |
|
Polimeri Europa Edistir R 540E Polystyrene
HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics IS..
|
|||
| Mold Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | |
|
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Mold Temperature | 20.0 - 120 °C | 68.0 - 248 °F | Injection Molding |
|
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**)
Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Advanced Elastomer Systems VistaFlex® 911-B Thermoplastic Rubber
(discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
|
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
|
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1047D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
|
Gromax 1155LL TPE
1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
|
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
|
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
LATI Latistat 52/7-02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
SK Chemicals SKYTHANE® S360D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Covestro Desmopan® DP 1080A Polyurethane
injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Covestro Desmopan® DP 3660DU Polyurethane
Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Covestro Desmopan® W DP 85085A Polyurethane
injection molding gradeno yellowing under the action of UV lightimproved microbial resistancegood low-temperature flexibilityImproved hydrolysis resistanceApplicationautomotive interior applications..
|
|||
| Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
|
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
|
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
|
BASF Elastollan 1185 A W TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
|
BASF Elastollan C 65 A HPM TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
|
BASF Elastollan 1185 A WM TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
|
BASF Elastollan 598 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri..
|
|||
| Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
|
BASF Elastollan S 85 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced
Polyurethane (PUR) based compound. Glass fibers. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
|
|||
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
|
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||