Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Multibase Multi-Pro® 4010 M Polypropylene
Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Multibase Multi-Pro® 4017 C Polypropylene
Calcium Carbonate Filler, 40% by weight.Features:Stiffness, Good Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Multibase Multi-Pro® 2003 TI Polypropylene
Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Mold Temperature 48.9 - 65.6 °C
120 - 150 °F
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 54.4 - 65.6 °C
130 - 150 °F
PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled  (discontinue
Description/Features:Glass/Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 54.4 - 65.6 °C
130 - 150 °F
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-1934G Styrenic Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 1581Forms: Pellets Proces..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2596C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2635D Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2717B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Inject..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
Mold Temperature 30.0 - 65.6 °C
86.0 - 150 °F
A. Schulman COMTUF® 420 Impact Modified PBT
Information provided by A. Schulman.
Mold Temperature 30.0 - 65.6 °C
86.0 - 150 °F
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Mold Temperature 30.0 - 65.6 °C
86.0 - 150 °F
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT
Information provided by A. Schulman.
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2069B Thermoplastic Elastomer
Uses: Caps; Food Packaging; Liners Pellets Processing Method: Extrusion; Injection Molding; Press Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmIn..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2683D Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Mold Temperature 30.0 - 65.6 °C
86.0 - 150 °F
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT
Information provided by A. Schulman.