Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Eurotec
Trade Name Tecolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Elongation at Break >= 200 %
>= 200 %
ISO 527
Tensile Modulus 0.750 GPa
109 ksi
ISO 527
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Processing Properties Metric English Comments
Processing Temperature 200 - 240 °C
392 - 464 °F
Feed Temperature <= 60.0 °C
<= 140 °F
Throat
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Hold Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Medium - Fast