Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 1020 C Polypropylene Calcium Carbonate Filler, 10% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 1505 R Polypropylene Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2004 R Polypropylene Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided .. |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2005 RCI Polypropylene Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided .. |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2010 M Polypropylene Mica Filled, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2516 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult.. |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2518 TU Polypropylene Talc Filled, 25% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3011 CHI Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3012 RC Polypropylene Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3014 XUGW Polypropylene Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3018 TU Polypropylene Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4005 M Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4008 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4012 TH Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4518 CUW Polypropylene Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2003 TI Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4005 MI Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 4007 XGS Polypropylene Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase |