Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 FRC 1 PA6 with flame retardant Features: Determined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material p.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Average value: 50.7 °C Grade Count:30 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Mold Temperature | 25.0 - 70.0 °C | 77.0 - 158 °F | Injection |
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals Introduction: IROGRAN A95K 4640 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection Molding |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Start Point: 60°C |
Kingfa PA66-R0N Flame Retardant PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelay, bobbins, plugsHousehold appliance partsE & E partsIn.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection Molding |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection Molding |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Mold Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical HI855S PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Injection Molding |
LG Chemical LUPOY GP5006BH PC/ABS, Heat Resistance, Impact Strength Description: Injection Molding, PC/ABS, Heat Resistance, Impact Strength, High ToughnessApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Start Point: 60°C |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Start Point: 60°C |
Kingfa PA6-T25 25% Mineral Filled PA6 Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Mold Temperature | 55.0 - 70.0 °C | 131 - 158 °F | |
Ecomass® 705ZC75 Stainless Steel Filled ABS Nontoxic Alternative to traditional metals, weighting and balancing applicationsModerate Specific GravityStainless Steel Powder Filled ABSInformation provided by Technical Polymers |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan 590 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan C 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan SP 852 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection molding |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |