| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 265 - 275 °C | 509 - 527 °F | |
|
NHEP Spectron™ E5469 Nylon 66, 33% Glass Fiber
Natural color. E5469 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informat..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | |
|
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | |
|
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | |
|
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | |
|
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ..
|
|||
| Nozzle Temperature | 185 - 275 °C | 365 - 527 °F | Average value: 234 °C Grade Count:22 |
|
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
|
|||
| Nozzle Temperature | 250 - 275 °C | 482 - 527 °F | Average value: 264 °C Grade Count:4 |
|
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact
Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact
Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
|
|||
| Nozzle Temperature | 250 - 275 °C | 482 - 527 °F | Injection Molding |
|
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage
Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GP5006BH PC/ABS, Heat Resistance, Impact Strength
Description: Injection Molding, PC/ABS, Heat Resistance, Impact Strength, High ToughnessApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY HG5000B PC/ABS, Heat Resistance
Description: Injection Molding, PC/ABS, High Gloss, Heat Resistance, High FlowApplication: E&E (housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY HR5007AE PC/ABS, High Impact
Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY NS5000 PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 235 - 275 °C | 455 - 527 °F | Injection Molding |
|
LG Chemical LUPOY SG5009F PC/ABS
Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | |
|
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc.
|
|||
| Nozzle Temperature | 270 - 275 °C | 518 - 527 °F | |
|
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy
Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def..
|
|||
| Nozzle Temperature | 265 - 275 °C | 509 - 527 °F | |
|
Lehmann & Voss LUVOCOM® 1800-7432 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Nozzle Temperature | 265 - 275 °C | 509 - 527 °F | |
|
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
|
|||
| Nozzle Temperature | 265 - 275 °C | 509 - 527 °F | |
|
Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact
Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9..
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | |
|
Solvay TECHNYL® A 52 G1 MX 20 PA66, Eh 0
Description: TECHNYL A 52 G1 MX20 is a Polyamide 6.6 glow wire resistant, reinforced with mineral fillerColors: it is marketed in black color.Available in: Latin AmericaMain Properties: ?Glow wire r..
|
|||
| Nozzle Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
|
LG Chemical LUPOY NS5000C PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi..
|
|||