Processing Properties Metric English Comments
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Nozzle Temperature 185 °C
365 °F
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Nozzle Temperature 185 °C
365 °F
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Nozzle Temperature 185 °C
365 °F
Termopol Termoton® V2GA1065A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Nozzle Temperature 185 °C
365 °F
Termopol Termoton® V6GA3075A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane
Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
Nozzle Temperature 185 - 205 °C
365 - 401 °F
Extrusion
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
Injection
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Injection Molding
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon.
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Injection Molding
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon.
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Injection Molding
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Nozzle Temperature 185 - 215 °C
365 - 419 °F
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 85 AB Thermoplastic Polyurethane
Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 92 AB Thermoplastic Polyurethane
Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma..
Nozzle Temperature 185 - 200 °C
365 - 392 °F
Lubrizol Estane® S392A Thermoplastic Polyurethane
Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow ..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Injection
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer
Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer
Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer
Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Nozzle Temperature 185 - 210 °C
365 - 410 °F
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Nozzle Temperature 185 - 220 °C
365 - 428 °F
Injection
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
Nozzle Temperature 185 °C
365 °F
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..