Polymer Property : Front Barrel Temperature = 302 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled
PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Front Barrel Temperature 279 - 302 °C
535 - 575 °F
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Front Barrel Temperature 279 - 302 °C
535 - 575 °F
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Front Barrel Temperature 279 - 302 °C
535 - 575 °F
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Front Barrel Temperature 277 - 302 °C
530 - 575 °F
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive..
Front Barrel Temperature 279 - 302 °C
535 - 575 °F
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled
PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade
PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Front Barrel Temperature 260 - 302 °C
500 - 575 °F
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy
General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC20NBR Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Front Barrel Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC721HFR Molding Grade PC
Information provided by Star Plastics, Inc.
Front Barrel Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC721HFR Molding Grade PC High Flow with Release
Information provided by Star Plastics, Inc.
Front Barrel Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC7523R Molding Grade PC
Information provided by Star Plastics, Inc.
Front Barrel Temperature 279 - 302 °C
535 - 575 °F
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 279 - 302 °C
535 - 575 °F
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 277 - 302 °C
530 - 575 °F
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.