| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced
Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced
Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-GP1 General Purpose Nylon 66
General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized
General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-MD1 Nylon 66, 1% MoS2
Nylon 66, 1% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced
Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
|
|||
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized
Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow
Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
|
|||
| Front Barrel Temperature | 277 - 302 °C | 530 - 575 °F | |
|
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
|
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
|
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 277 - 293 °C | 531 - 559 °F | |
|
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced
Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified
Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM1-[color]-H Nylon 66, Medium Impact Modified, Heat Stabilized
Nylon 66, Medium Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Ny..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM1-[color]H Nylon, Medium Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-MD2 Nylon 66, 2% MoS2
Nylon 66, 2% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
|
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
|
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
|
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
|
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR
Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req..
|
|||
| Front Barrel Temperature | 277 °C | 530 °F | |
|
Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled
Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistanc..
|
|||