Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 303 Natural FA PA66, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 303 Natural FA PA66, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe Product Applications: TECHNYL® A 303 Natural FA offers three main advantages: high impact resistance at low humidity levels, good rigidity, and excellent compression resistance. This grade is particularly suitable for extrusion of plates and profiles. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Water Absorption 1.69 %

@Temperature 23.0 °C,
Time 86400 sec
1.69 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527 Type 1A
Tensile Strength, Yield 84.0 MPa
12200 psi
ISO 527 type 1 A
Elongation at Break 30 %
30 %
ISO 527 Type 1A
Tensile Modulus 3.00 GPa
435 ksi
ISO 527 Type 1A
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ISO 11357
Processing Properties Metric English Comments
Feed Temperature 240 - 250 °C
464 - 482 °F
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Compression Zone 240-260°C
Draw-plate temperatures 260-270°C