Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Front Barrel Temperature | 270 - 310 °C | 518 - 590 °F | |
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi.. |
|||
Front Barrel Temperature | 270 - 310 °C | 518 - 590 °F | |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |