Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 216 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 2004 R Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 4012 X Platinum Polypropylene
Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P103-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Battery traysFender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade
Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 216 - 235 °C
420 - 455 °F
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring..
Front Barrel Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Front Barrel Temperature 216 °C
420 °F
TPI Porene® ABS-AN450 Flame Retardant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 216 - 266 °C
421 - 511 °F
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer
Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume..
Front Barrel Temperature 216 - 266 °C
420 - 510 °F
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s..
Front Barrel Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app..
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
LTL Color Compounds ColorFast® GPA300 ABS
Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
LTL Color Compounds ColorFast® GPA300X ABS
Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po..
Front Barrel Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene  (discontinued **)
Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L..
Front Barrel Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene  (discontinued **)
High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of ..
Copyright © lookpolymers.com All Rights Reserved