| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded |
| Manufacturer | Ravago Manufacturing Americas, LLC |
| Trade Name | Hylac® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ravago Manufacturing Americas Hylac® GP74 ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
| Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| 8.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 109 | 109 | ASTM D785 |
| Tensile Strength, Yield | 46.5 MPa | 6750 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Tensile Modulus | 2.72 GPa | 395 ksi | ASTM D638 |
| Flexural Yield Strength | 75.8 MPa | 11000 psi | ASTM D790 |
| Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
| Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 0.25 in; ASTM D256 |
| 2.24 J/cm | 4.20 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 93.6 µm/m-°C @Temperature -40.0 - 176 °C |
52.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 95.6 °C | 204 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
| Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
| Flammability, UL94 | HB | HB | 0.0590 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 179 - 199 °C | 355 - 390 °F | |
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| Front Barrel Temperature | 216 - 235 °C | 420 - 455 °F | |
| Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
| Melt Temperature | 241 °C | 465 °F | Aim |
| Mold Temperature | 48.9 - 60.0 °C | 120 - 140 °F | |
| Moisture Content | <= 0.10 % | <= 0.10 % | |
| Injection Pressure | 5.86 - 6.89 MPa | 850 - 1000 psi | |
| Back Pressure | 0.483 - 0.965 MPa | 70.0 - 140 psi | |
| Shot Size | 40 - 80 % | 40 - 80 % | |
| Screw Speed | 50 - 90 rpm | 50 - 90 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure | 710 to 850 psi | |
| Injection Rate | Slow-Moderate |