Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well suited for consumer goods and industrial applications requiring non-slip/soft dry-touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK40B can be overmolded to PC, ABS, PC/ABS, Acrylic, HIPS, copolyester, various grades of polyamide, and more.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength 2.96 MPa
429 psi
ASTM D412
Elongation at Break 338 %
338 %
ASTM D412
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 210 - 216 °C
410 - 420 °F
Front Barrel Temperature 216 - 266 °C
420 - 510 °F
Nozzle Temperature 227 - 277 °C
440 - 530 °F
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Injection Velocity 25.4 - 127 mm/sec
1.00 - 5.00 in/sec
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi