Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK60X can be overmolded to polycarbonate, ABS, PC/ABS, and various grades of nylon 6 and 6/6.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
ASTM D2240
Tensile Strength, Yield 8.30 MPa
1200 psi
ASTM D412
Elongation at Break 541 %
541 %
ASTM D412
100% Modulus 0.00180 GPa
0.261 ksi
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 210 - 216 °C
410 - 421 °F
Front Barrel Temperature 216 - 266 °C
421 - 511 °F
Nozzle Temperature 227 - 277 °C
441 - 531 °F
Mold Temperature 27.0 - 49.0 °C
80.6 - 120 °F
Injection Velocity 25.0 - 127 mm/sec
0.984 - 5.00 in/sec
Back Pressure 0.520 - 1.21 MPa
75.4 - 175 psi
Users viewing this material also viewed the following: