Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 155 - 165 °C | 311 - 329 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Processing Temperature | 155 - 165 °C | 311 - 329 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | Mixture Zone |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Average value: 150 °C Grade Count:8 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Processing Temperature | 150 - 165 °C | 302 - 329 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 10 C Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 10 EC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 10 SC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 25 C Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 150 - 165 °C | 302 - 329 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7312 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |