Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 0.5-1 hr. |
Von Roll Isola IMI Varnish 271 Spirit Gum Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 0.5-1 hr. |
Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 19°C. Average solids: 60%. Usage Notes: Use with IMI 74010 hardener for final coat over field coils, windings, and heavy duty motors. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 6-18 hr. May also be cured for shorter time at higher temperatures. |
Von Roll Isola IMI E-Solder® 3012 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 180 °C | 275 - 356 °F | Average value: 162 °C Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |