| Category | Polymer , Thermoset , Epoxy , Epoxy Molding Compound |
| Manufacturer | Cosmic Plastics |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Cosmic Plastics CP7311 Epoxy Molding Compound.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.00 g/cc | 0.0723 lb/in³ | |
| Water Absorption | 0.20 % | 0.20 % | 48 hrs, 50°C |
| Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | typical. |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 138 - 207 MPa | 20000 - 30000 psi | |
| Flexural Strength | 345 MPa | 50000 psi | |
| Compressive Strength | 241 MPa | 35000 psi | |
| Izod Impact, Notched | 21.0 J/cm | 39.3 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 243 °C | 469 °F | Heat Distortion temperature |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |