Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East) CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific) Super high impact ABS. Good low temperature toughness. High gloss. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East) CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.60 mm |
140 °F @Thickness 0.0630 in |
UL746B |
Ineos ABS Lustran® 256 Extrusion, Blending
(discontinued **) A natural, medium-flow, medium-impact extrusion grade of ABS. It is used for blending with other Lustran ABS virgin and regrind materials to optimize cost and performance.Properties tested in trans.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.60 mm |
140 °F @Thickness 0.0630 in |
UL746B |
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **) A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.00 - 1.10 mm |
140 °F @Thickness 0.0394 - 0.0433 in |
|
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL746B |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL746B |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific. |
|||
UL RTI, Mechanical without Impact | 60.0 - 80.0 °C | 140 - 176 °F | Average value: 63.3 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |