| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.160 % | 0.160 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.60 % | 0.60 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
| Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 90 | 90 | ISO 2039-2 |
| Tensile Strength at Break | 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 |
| 45.0 MPa | 6530 psi | 5 mm/min; ISO 527 | |
| 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | 5 mm/min; ISO 527 |
| 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 | |
| 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 45 % | 45 % | Type I, 50 mm/min; ASTM D638 |
| 50 % | 50 % | 50 mm/min; ISO 527 | |
| 60 % | 60 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 5.0 % | 5.0 % | Type I, 50 mm/min; ASTM D638 |
| 5.0 % | 5.0 % | 5 mm/min; ISO 527 | |
| 5.0 % | 5.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D638 |
| 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 80.0 MPa | 11600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 80.0 MPa | 11600 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | Izod Impact, double-gated, 23°C; SABIC Method |
| 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 | |
| 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
| 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
| 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 | |
| Impact Test | 70.0 J | 51.6 ft-lb | Multiaxial Impact; ISO 6603 |
| Taber Abrasion, mg/1000 Cycles | 70 | 70 | CS-17, 1 kg; SABIC Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C177 |
| 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 | |
| Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 115 °C @Thickness 3.20 mm |
239 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
| 114 °C | 237 °F | Rate B/50; ISO 306 | |
| 116 °C | 241 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
| UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
UL 94 |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
UL 94 | |
| Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D257 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.9 @Frequency 50.0 - 60.0 Hz |
2.9 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
| 36.0 kV/mm @Thickness 0.800 mm |
914 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 | |
| Dissipation Factor | 0.010 @Frequency 50.0 - 60.0 Hz |
0.010 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
| 0.011 @Frequency 1.00e+6 Hz |
0.011 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | passes | IEC 60695-10-2 |