Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANAMID 66 A12^ F35 NH9 Nylon 66, Glass Fiber Reinforced, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | ISO 75/Bf |
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | ISO 75/Bf |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66 LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp RF005 PA 66 (Asia Pacific) LNP* Thermocomp* RF005 is a compound based on Nylon 66 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66 LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66 LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AE is a compound based on PA 66 rsin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 622 Nylon 6/6, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Dry; ASTM D648 |
Asahi Kasei Leona® 14G15 15% Glass Filled Nylon 66 15% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Heater tanks, fuel injectors, ABS sensors, and other under-the-hood automotive parts Information provided by Asahi Kasei |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | ASTM D648 |
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |