Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANAMID 66 A12^ F35 NH9 Nylon 66, Glass Fiber Reinforced, Flame Retardant, Halogen Free

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled , Nylon 66, 40% Glass Fiber Filled
Manufacturer Polykemi AB
Trade Name SCANAMID 66
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANAMID 66 A12^ F35 NH9 Nylon 66, Glass Fiber Reinforced, Flame Retardant, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Filler Content 35 %
35 %
±2%; Polykemi
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 165 MPa
<= 23900 psi
ISO/R527
Elongation at Break 3.0 %
3.0 %
ISO/R527
Flexural Strength <= 270 MPa
<= 39200 psi
ISO 178
Flexural Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 244 °C
471 °F
120°C/h; ISO 75/1
Vicat Softening Point >= 250 °C

@Load 1.00 kg
>= 482 °F

@Load 2.21 lb
50°C/h; ISO 306
>= 250 °C

@Load 5.001 kg
>= 482 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
IEC 695-2-1