| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.37 g/cc | 0.0495 lb/in³ | DAM; ISO 1183 |
| Filler Content | 30 % | 30 % | DAM |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 124 MPa @Temperature 23.0 °C |
18000 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 187 MPa @Temperature 23.0 °C |
27100 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 3.0 % @Temperature 23.0 °C |
3.0 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 4.5 % @Temperature 23.0 °C |
4.5 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 7.00 GPa @Temperature 23.0 °C |
1020 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 9.90 GPa @Temperature 23.0 °C |
1440 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -40.0 °C |
3.33 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
| 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
| Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
| 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
| 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
| 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 258 °C | 496 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | DAM; ISO 75-1/-2 |
| UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
DAM; UL 746B |
| 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
DAM; UL 746B | |
| UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
DAM; UL 746B |
| 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
DAM; UL 746B | |
| 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
DAM; UL 746B |
| 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
DAM; UL 746B | |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
DAM; IEC 60695-11-10 |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
DAM; UL94 | |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; UL94 | |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; UL94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 400 V @Temperature 23.0 °C |
400 V @Temperature 73.4 °F |
DAM; UL 746A |
| 400 - 600 V @Temperature 23.0 °C |
400 - 600 V @Temperature 73.4 °F |
DAM |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 295 °C | 563 °F | DAM; Optimum |
| 285 - 305 °C | 545 - 581 °F | DAM | |
| Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | DAM |
| 100 °C | 212 °F | DAM; optimum | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black Color | DAM |
| Drying Recommended | Yes, if moisture content of resin exceeds recommended level | DAM |
| Filler | Glass Reinforced | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 66 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA66-GF30< | ISO 11469; DAM |
| Polymer Family | Polyamide | DAM |
| Polymer Type | PA66 | DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Glass Reinforced Resins | DAM |
| Resin Identification | PA66-GF30 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |