Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® EX75 ABS Multi-purpose, extrusion ABS providing a favorable balance of engineering properties. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A flame retardant, novolac-hardened epoxy molding compound recommended for semiconductor packages that are not stress sensitive. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C | 45.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP ICL34 PA6.12 LNP* LUBRICOMP* ICL34 is a compound based on Nylon 6/12 containing 20% Carbon Fiber, 15% PTFE. Added features include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features include Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -20.0 - 150 °C |
45.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -20.0 - 150 °C |
45.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10 LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive. |