Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific)

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name GELOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 10 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
21.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
21.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength at Break 44.0 MPa
6380 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 36 %
36 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 3.7 %
3.7 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 3.03 GPa
439 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 3.04 J/cm
5.70 ft-lb/in
ASTM D256
0.690 J/cm

@Temperature -30.0 °C
1.29 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
ASTM D3763
33.0 J

@Temperature 23.0 °C
24.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 3.20 mm
194 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 121 °C
250 °F
Rate B/50; ASTM D1525
Flame Spread 39.0 mm/min

@Thickness 1.00 mm
1.54 in/min

@Thickness 0.0394 in
FMVSS 302
Optical Properties Metric English Comments
Gloss 98 %
98 %
untextured, 60 degrees; ASTM D523
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved