Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Nilit FRIANYL B63 KG20 Nylon 6 for injection molding, 20% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lucite International Diakon® CLH952 Acrylic Polymer Information provided by Lucite International |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lucite International Diakon® CMG314V Acrylic Polymer Information provided by Lucite International |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lucite International Diakon® Frost 952 80 Acrylic Polymer Information provided by Lucite International |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Lucky EF-940 Acrylic, Injection/Extrusion Grade Extrusion and injection grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capa.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RB003 PA 66 (Europe-Africa-Middle East) 15% glass beads filled polyamide 66 injection moulding resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Unitika BV2120 PA66, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178-93 |
Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178-93 |
Wellman Wellamid® FR22F-NBK3 Flame Retardant Nylon 66 Description: Flame Retardant Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2mm/min; ISO 178 |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM-D790 |
Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber 20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP H 1080 T6 T D Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerGood physical and mechanical characteristics, high thermal stability, detergent resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | dry; ISO 178 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO Data |
BASF Ultramid® 1310-11 NF2001 PA66 (Dry) Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Flexural Modulus | 3.20 - 6.21 GPa | 464 - 900 ksi | Average value: 5.01 GPa Grade Count:25 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Flexural Modulus | 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF002R PES (Europe-Africa-Middle East) LNP* Thermocomp* JF002R is a compound based on Polyethersulfone resin containing Glass Fiber, Glass Bead. Added features of this material include: Mold Release. |